چکیده
|
In recent years, increasing research efforts have focused on assessing the potential of polymeric nanofibers to improve the bio-availability and stability of active agents via encapsulation. In this study, gelatin (GL) and octenyl succinic anhydride-modifiedstarch (OS-ST) were employed to fabricate GL/OS-ST nanofibers incorporating 5% (v/v) sage extract (SE). GL/OS-ST solutionswith ratios of 100/0, 90/10, 70/30, 60/40, and 50/50 (w/w) were prepared for electrospinning. The results showed that increasingthe OS-ST content decreases both the viscosity of the blended solution and the nanofiber diameter, with the latter reaching ap-proximately 231.62 nm. Fourier transform infrared (FTIR) spectroscopy confirmed hydrogen bonding between GL and OS-ST,as well as the successful incorporation of SE into the nanofibers. X-ray diffraction (XRD) analysis indicated that SE incorpora-tion did not induce crystallization in the polymer chains, and that all nanofibers exhibited amorphous structures, confirmingthe homogeneous dispersion of SE. Antioxidant activity assays demonstrated sustained SE release over 48 h, achieving a radicalscavenging activity of 72.3% ± 3%. Overall, the prepared nanofibers effectively retarded SE release. The optimal GL/OS-ST ratio(70:30) produced uniform fibers with high encapsulation efficiency (87.5% ± 2.1%), underscoring the potential of these nanofibersas delivery systems for bioactive compounds in functional foods.
|