Fungal leaching of valuable metals from a power plant residual ash using Penicillium simplicissimum: Evaluation of thermal pretreatment and different bioleaching methods
Type
JournalPaper
Keywords
Bioleaching PPR ash Thermal pretreatment Vanadium recovery Penicillium simplicissimum
Year
2016
Journal WASTE MANAGEMENT
DOI
Researchers Payam Rasoulnia ، Seyyed Mohammad Mousavi ، Seyed Omid Rastegar ، hamidreza azargoshasb

Abstract

Each year a tremendous volume of V-Ni rich ashes is produced by fuel oil consuming power plants throughout the world. Recovery of precious metals existing in these ashes is very important from both economic and environmental aspects. The present research was aimed at investigating bioleaching potential of Penicillium simplicissimum for the recovery of metals from power plant residual ash (PPR ash) using different bioleaching methods such as one-step, two-step, and spent-medium bioleaching at 1% (w/v) pulp density. Furthermore, the effects of thermal pretreatment on leaching of V, Ni, and Fe, as major elements present in PPR ash, were studied. Thermal pretreatment at various temperatures removed the carbonaceous and volatile fraction of the ash and affected the fungal growth and metal leachability. The highest extraction yields of V and Ni were achieved for the original PPR ash, using spent-medium bioleaching in which nearly 100% of V and 40% of Ni were extracted. The maximum extraction yield of Fe (48.3%) was obtained for the pretreated PPR ash at 400 C by spent-medium bioleaching. In addition, the fungal growth in pure culture was investigated through measurement of produced organic acids via high performance liquid chromatography (HPLC). Chemical leaching experiments were performed, using commercial organic acids at the same concentrations as those produced under optimum condition of fungal growth (5237 ppm citric, 3666 ppm gluconic, 1287 ppm oxalic and 188 ppm malic acid). It was found that in comparison to chemical leaching, bioleaching improved V and Ni recovery up to 19% and 12%, respectively. Moreover, changes in physical and chemical properties as well as morphology of the samples utilizing appropriate analytical methods such as XRF, XRD, FTIR, and FE-SEM were comprehensively investigated.